有机硅稀释剂®是一种非反应性硅油,可降低锡固化(缩合聚合)或铂金固化(加成)硅胶产品的混合粘度。
*Silicone Thinner® is added as a percentage of the total Part A+Part B rubber system. An accurate gram scale must be used. Weigh out and pre-mix required amount of Silicone Thinner® with Part A of silicone rubber before adding Part B. Mix all components thoroughly and vacuum as directed on mold rubber technical bulletin.
It is not recommended to exceed 10% by weight of total system (A+B).
Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.