Example - Ecoflex 00-30 (1:1 Mix Ratio): To reduce the demold time of Ecoflex 00-30 from 4 hours to 1 hour, add 40 grams of accelerator to 1000 grams of Ecoflex 00-30 Part A. Mix thoroughly for one minute, making sure that you scrape the sides and bottom of your container several times. Next, add 1000 grams of Part B and mix thoroughly for one minute, again making sure that you scrape the bottom and sides of your container several times. Do not delay between mixing and pouring, as your pot life is about 10 minutes. In about 1 hour, the rubber mold can be removed from the original model.
Example – Smooth Sil 940 (10:1 Mix Ratio): To reduce the demold time of Smooth-Sil 940 from 16 hours to 2.5 hours, add 20 grams ofaccelerator to 1000 grams of Smooth-Sil 940 Part A. Mix thoroughly for one minute, making sure that you scrape the sides and bottom of your container several times. Next, add 100 grams of Part B and mix thoroughly for one minute, again making sure that you scrape the bottom and sides of your container several times. Do not delay between mixing and pouring, as your pot life is about 10 minutes. In about 3 hours, the rubber mold can be removed from the original model.