Psycho Paint

PsychoPaint®为多用途且易于使用的铂金固化上色涂层硅胶,用于提升特殊效果和修复工匠、娃娃制造商等轻松地为其铂金固化硅胶创作品创建颜色效果。产品为双组分半透明的铂金固化硅胶,用于制作彩色硅胶涂层。达到所需的颜色后,Psycho Paint®用溶剂稀释,使用喷笔薄层喷涂到模型表面(由DragonSkin®、Ecoflex®或其他铂金硅胶制成)。也可以通过刷子涂刷。

特征

彩色Psycho Paint®硅胶与模型表面粘合并具有良好的耐磨性。产品非常坚固,随着模型拉伸和弯曲,不会开裂或脱落。需要临时将硅胶面罩、假体装置或其他创作粘附到您的皮肤上吗?询问Smooth-On经销商关于Slacker®触变软化剂和Skin-Tite®皮肤粘合剂。

说明

Safety - Use in a properly ventilated area (“room size” ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk. Wear vinyl gloves only. Latex gloves will inhibit the cure of the rubber.
 

Store and use all products at room temperature (73°F / 23°C). This product has a limited shelf life and should be used as soon as possible. Silicone surfaces to be painted can only be Platinum (addition) cured systems. For optimum results the silicone skin/surface, should be painted as soon as possible after demolding. We recommend that the cured piece to be painted be no more than 2 days old.

Clean All Surfaces That Will Contact Psycho Paint® - All surfaces to be painted, need to be free of any contaminants (especially mold release). If necessary, clean all surfaces with solvent (NOVOCS™ Zero VOC Solvent, Toluene, Xylene, or Naptha), and allow to dry before painting.


Measuring Is Done By Volume - The recommended mix ratio is 100 Parts A + 100 Part B + 200-500 Parts Solvent depending on your application (hand painting vs. airbrushing).

Adding Color To Psycho Paint® - Silc Pig® silicone pigments are compatible with Psycho Paint®. There are several colors to choose from, and you can mix colors to create custom colors. The most accurate way to add pigment is by weight (using a gram scale). We recommend beginning by pre-mixing 2% pigment by weight to Part B and pre-mixing thoroughly. Do not exceed a 5% pigment load of the total weight (A+B). You can also use powdered cosmetic pigments to color Psycho Paint®, however a compatibility test is recommended.

Adding Solvent - Once a desirable color effect is attained, add an equal amount of Psycho Paint® Part A. Next, add 200-500 Parts of solvent. Smooth-On’s NOVOCS™ Zero VOC Solvent is recommended. Toluene, Xylene or Naptha are also suitable. Observe all safety precautions when handling combustible or flammable solvents. Mix thoroughly to a uniform color (no streaks).


Applying Psycho Paint® Using An Air Brush - Dispense mixture into air brush siphon cup / gravity cup. Apply thin layers of paint to the model’s surface until the desired color effect is attained.

Brushing Onto A Platinum Silicone Appliance Or Model - Make sure all surfaces are clean. Add the desired amount of Silc Pig® pigment to Psycho Paint® Part B and mix thoroughly. Add an equal amount of Psycho Paint® part A and mix thoroughly. Add solvent if desired. You can then apply Psycho Paint® with a brush. A common application technique is to use a “stippling” effect.

Important - Pot life of undiluted Psycho Paint® (without solvent) is 20 minutes at room temperature.

Curing - Undiluted Psycho Paint® will cure at room temperature in 2 hours. Cure time can be reduced with heat (oven or heat gun). Do not expose to over 212°F/100°C. If heat curing, make sure that all solvents have evaporated from model’s surface, before applying heat.

介绍产品制作工艺的文章

使用Psycho Paint为铂金固化硅胶上色

使用Psycho Paint为铂金固化硅胶上色

分步视频概述Psycho Paint硅胶涂料基材的使用和铂金固化硅胶浇注件表面的上色

› 查看介绍文章

使用Dragon Skin硅胶制作响尾蛇道具

使用Dragon Skin硅胶制作响尾蛇道具

Blair Benjamin为独立电影项目制作响尾蛇道具

› 查看介绍文章

使用NOVOCS高光和哑光有机硅溶剂

使用NOVOCS高光和哑光有机硅溶剂

视频概述如何使用NOVOCS高光和哑光溶剂,及两者的主要区别

› 查看介绍文章