THI-VEX®特别适用于Smooth-On硅胶的增稠,用于垂直表面应用(制作刷涂模具)。通过改变添加的THI-VEX®的添量,可以获得不同的粘度。
 
THI-VEX®以A组份的百分比添加,并且必须与A组分和B组分充分混合。

特征

说明

THI-VEX® will not work with Mold Max® 40 or Mold Max® 60 silicones.
 

Safety - Use in a properly ventilated area (“room size” ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk.

Store and use material at room temperature (73°F/23°C). This product has a limited shelf life and should be used as soon as possible.

MEASURING & MIXING - If using Mold Max®, the brush-on mold process can be shortened with Fast Cat® 30 catalyst or Accel-T® cure accelerator. Because silicones have a long pot life, time between coats can be 2–3 hours. Adding Fast Cat® 30 catalyst or Accel-T® cure accelerator will accelerate the brush-on mold making process down to a matter of hours.

Mixing - Add desired amounts of THI-VEX® to material and mix thoroughly. Important: Be sure to scrape the sides and bottom of the mixing container several times while mixing. Be aware of your working time. Note: results may differ due to variables in temperature, humidity, etc.

Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.