Derma-tac™

Derma-tac™

Derma-tac™硅胶假体粘合剂为压敏粘合剂,设计用于临时粘合硅胶和乳胶化妆假肢器具到皮肤。
 
根据OECD测试指南439,Derma-tac™具有皮肤安全性,并由独立实验室认证。测试用于以确定材料的皮肤敏感性。粘合剂为低气味的化妆品级配方,无刺激性。
 
注意:如果是粘合不是秃顶盖帽塑料膜和Ecoflex™硅胶制作的装置,使用Skin Tite™皮肤安全硅胶粘合剂的粘合性更好。

特征

说明

PREPARATION...
 

Important: Shake Derma-tac™ container well before using.

Preparation - Clean the skin with soap and water to remove any oils which may affect the bond of the Derma-tac™ adhesive. Allow skin to dry completely.


APPLICATION & REMOVAL...
Acclerating / Lowering Viscosity – Drying time can be reduced with NOVOCS Gloss Silicone Solvent. Adding 10% NOVOCS gloss by weight will lower viscosity and reduce dry time by about ½.
Application - Derma-tac™ adhesive can be applied using a cotton swab, non-latex makeup sponge or suitable makeup brush. Apply adhesive to the surface of the skin or appliance. When applying on areas of high stretch or movement, such as around the mouth, adhesive can be applied to both the skin and the appliance.
Important: Allow Derma-tac™ to evaporate completely. This adhesive will not work unless it has thoroughly dried. Once Derma-tac™ has dried, press the makeup appliance in place. Derma-tac™ is a pressure sensitive adhesive, the firmer you press, the better the adhesive bond.
Appliance Removal Using Derma-tac™ Remover - Apply Derma-tac™ Remover using a cotton swab, cotton ball or suitable makeup brush. Work the Derma-tac™ remover under the edges of the appliance and onto the skin. work the appliance away from the skin slowly, taking particular care around the eyes, nose and mouth.
Once the Derma-tac™ has been removed, the skin should be cleaned and moisturized using a cosmetic cleanser and moisturizer.

介绍产品制作工艺的文章

用Derma-tac粘帖硅胶器具

用Derma-tac粘帖硅胶器具

了解如何使用Derma-tac和Derma-tac去除剂应用硅胶假体

› 查看介绍文章