Derma-tac™ Remover

Derma-tac™ Remover

Dermatac™ Remover为易于使用的单组分液体,能够溶解Derma-tac™ 并有助于从皮肤上去除装置。
 
Derma-tac™去除剂皮肤安全,并通过独立实验室根据OECD测试指南439进行认证。测试用以确定材料的皮肤敏感性。产品为低气味化妆品级配方,无刺激性。

特征

说明

PREPARATION...
 

Important: Shake Derma-tac™ container well before using.

Preparation - Clean the skin with soap and water to remove any oils which may affect the bond of the Derma-tac™ adhesive. Allow skin to dry completely.


APPLICATION & REMOVAL...
Acclerating / Lowering Viscosity – Drying time can be reduced with NOVOCS Gloss Silicone Solvent. Adding 10% NOVOCS gloss by weight will lower viscosity and reduce dry time by about ½.
Application - Derma-tac™ adhesive can be applied using a cotton swab, non-latex makeup sponge or suitable makeup brush. Apply adhesive to the surface of the skin or appliance. When applying on areas of high stretch or movement, such as around the mouth, adhesive can be applied to both the skin and the appliance.
Important: Allow Derma-tac™ to evaporate completely. This adhesive will not work unless it has thoroughly dried. Once Derma-tac™ has dried, press the makeup appliance in place. Derma-tac™ is a pressure sensitive adhesive, the firmer you press, the better the adhesive bond.
Appliance Removal Using Derma-tac™ Remover - Apply Derma-tac™ Remover using a cotton swab, cotton ball or suitable makeup brush. Work the Derma-tac™ remover under the edges of the appliance and onto the skin. work the appliance away from the skin slowly, taking particular care around the eyes, nose and mouth.
Once the Derma-tac™ has been removed, the skin should be cleaned and moisturized using a cosmetic cleanser and moisturizer.