Q-Ballz™

Q-Ballz™

Q-Ballz™为单组分液体,可用作秃顶盖帽塑料或用于封装硅胶假体用具。用丙酮稀释将材料用喷笔喷涂到模具中(或塑料头模具表面)形成薄膜。开封后尽快使用。

封装在Q-Ballz™中的硅胶假肢矫正装置的边缘可以用丙酮溶解掉。Q-Ballz™还可用于在合适的头型上制作光头帽。

特征

说明

WARNING - FLAMMABLE Liquid and vapor. Keep away from ignition sources and follow precautions for handling flammables.
 

Materials should be stored and used in a warm environment (73°F / 23°C). This material has a limited shelf life and should be used as soon as possible. Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk.
Important: Shake Q-Ballz™ Container Well Before Using.

FOR CREATING BALD CAPS:

  1. Apply a thin layer of release agent, such as Ease Release® 200 or petroleum jelly, to a bald cap head form.
  2. Stipple undiluted Q-Ballz™ thinly over the desired area of the bald cap head form.
  3. Allow at least 10 minutes of drying time between layers.
  4. Repeat steps 2-3 to build up an appropriate thickness. Generally, 5-10 layers are sufficient.
  5. Allow at least 2 hours for acetone to completely flash off before removing bald cap from the head form.
  6. Powder outside of bald cap using talcum powder.
  7. Remove bald cap from head form gently using a soft brush and talcum powder.
  8. Fine edges of the completed bald cap can be dissolved using acetone.

FOR USE AS AN ENCAPSULANT FOR SILICONE APPLIANCES:

  1. Apply a thin layer of release agent, such as Ease Release® 200 or petroleum jelly, to all surfaces of prosthetic mold.
  2. Thin Q-Ballz™ with acetone. Generally 3-4 parts acetone added to 1 part Q-Ballz™ is sufficient.
  3. Using an airbrush or other fine mist sprayer, spray a thin layer of thinned Q-Ballz™ over all mold surfaces
  4. Allow at least 10 minutes of drying time between layers.
  5. Repeat steps 3-4 to build up an appropriate thickness. Generally, 5-10 layers are sufficient.
  6. Fill mold using a silicone gel such as Ecoflex® Gel or Dragon Skin® softened with SLACKER®.
  7. Allow silicone gel to fully cure.
  8. Optional - spray 3-4 thin layers of thinned Q-Ballz™ over back of appliance.
  9. Demold silicone gel filled appliance with the assistance of a soft bush and talcum powder.
  10. Fine edges of the completed encapsulated appliance can be dissolved using acetone.