Free Form SCULPT®

Free Form SCULPT®

FreeFormory®SCULPT为双组分可雕刻环氧粘土,不需要烧制,可在短时间内自固化,达到极其坚硬耐用的状态,并几乎不会收缩。SCULPT比同类产品轻30%,可以更好地附着在垂直表面。用户可以更好地控制重量分布,雕刻更大、更牢固的作品。Free Form SCULPT具有超细颗粒尺寸,使用户能够使用工具或手成型更精确、雕刻更精细的细节。
 
镜面般的光泽表面可以通过固化前用水处理。

特征

最大可用性 - 只需添加水:可以在混合A + B组分时通过添加水来改变FreeForm®SCULPT的一致性和工作性。雕刻时,油灰表面可以用水抹光滑。
 
A和B组分用手等量混合。工作时间长达1.5小时,FreeForm®SCULPT可以在一夜之间固化成坚硬、刚性的环氧树脂,非常牢固并具有防水性。SCULPT容易通过添加SO-Strong颜色来制作大理石或其他效果。固化后的腻子容易用丙烯酸涂料上色。
 
FreeForm®SCULPT不含结晶硅(一种已知的致癌物)。可以安全地打磨、成形和涂漆。
 
用作修补胶,FreeForm®SCULPT可粘合自身和各种表面,包括木材、金属、玻璃、石材和混凝土。FreeForm®SCULPT甚至可以在水下固化

说明

Safety – Use in a properly ventilated area (“room size” ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk. Wear disposeable gloves. Use of a NIOSH approved respirator is recommended.

Preparation – Materials should be stored and used in at room temperature (73° F / 23° C). Mixing should be done in a wellventilated area. Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.

Applying A Release Agent – For releasing epoxy from non-porous surfaces such as resin, metal, glass etc., use Ease Release 200 or 205 (available from Smooth-On) to prevent adhesion.

This product is mixed by hand. You must wear disposable gloves when mixing this material.


Measuring - Free Form® SCULPT putty comes as two parts. Dispense equal amounts (golf ball size, for example) of Part A and Part B.

Mixing - Knead parts together aggressively to a uniform color and apply to surface. Immersing in water periodically will make Free Form® SCULPT more workable.

Pot Life/Working Time - This material is mass sensitive. The more material you mix at one time, the less time you have to work with it. Working tip; If mixing a large quantity, flatten putty with a rolling pin to reduce mass concentration and extend pot life.


Applying – Mixed Free Form® SCULPT is a dough that can be applied up to 2.5” (6.35 cm) thickness. Pot Life and Cure Time values are dependent on mass and ambient temperature. The greater the mass, the shorter the working time. Shrinkage will also be higher.

Free Form® SCULPT will gradually stiffen during its working life, changing its pliability. Add water periodically using a spray bottle to improve workability. It will be most adhesive within the first 30 minutes.


Use as a Sculpting Medium - Free Form® SCULPT can be applied to wire mesh armatures to create rigid forms for sculpting. Wire mesh for sculpting is available at most art supply stores.

If making a large sculpture, work in small sections and apply in layers to build up a suitable thickness. Putty can be rolled out between two sheets of wax-paper using a rolling pin.

Knead new sections with your fingers to bond the edges. Smooth surface of putty with water. Use water to keep sculpting tools from sticking to putty.

While Sculpting - Using a water misting spray bottle, mist water onto putty surface to maintain workability.

To Sculpt Fine Detail and Add Texture – Allow water to evaporate slightly. Putty will stiffen and allow sculpting of fine detail.


Curing - Free Form® SCULPT will reach full properties after 24 hours at room temperature. Cured epoxy is waterproof and can be sanded or machined. If machining or sanding, wear NIOSH approved particulate mask to prevent inhalation of particles.

Painting – Cured Free Form® SCULPT can be primed and painted with acrylic enamel paints. Let paint fully dry before handling.

Heat Resistance – Fully cured putty with a minimum thickness of ½” (1.27 cm) will resist temperatures up to 150° F / 65° C.


Removing Uncured Free Form® SCULPT - Remove as much uncured material from the surface as possible. Clean any residue with soap and water. Optional - Use E-POX-EE KLEENER® available from Smooth-On.

Shelf Life - In an unopened container, at 73° F / 23° C, shelf life is 2 years. Use entire contents as soon as possible after opening.

介绍产品制作工艺的文章

使用FreeForm SCULPT修复找到的稀有品

使用FreeForm SCULPT修复找到的稀有品

40多年来,蒂姆贝内特的爱好一直是在车库和庭院销售中寻找稀有品

› 查看介绍文章

Free Form SCULPT 环氧制作的雕塑上色演示

Free Form SCULPT 环氧制作的雕塑上色演示

Free Form SCULPT 可以永久上色-无需底漆

› 查看介绍文章

如何使用环氧油灰制作仿大理石笔

如何使用环氧油灰制作仿大理石笔

客户Jara A演示如何使用Free Form Sculpt制作仿大理石笔

› 查看介绍文章

使用Free Form Sculpt制作刚性大师

使用Free Form Sculpt制作刚性大师

Ryan Sparks专业为客户浇注精确真实的身体部位

› 查看介绍文章

用Free Form AIR &SCULPT环氧油灰雕塑

用Free Form AIR &SCULPT环氧油灰雕塑

用Free Form AIR &SCULPT环氧油灰雕塑演示

› 查看介绍文章