Store and use material at room temperature (73°F/23°C). This product has a limited shelf life and should be used as soon as possible.
SHAKE WELL BEFORE USING
Applying - Thoroughly clean your mold with Mold Cleaner 2508 or any suitable cleaner to remove all traces of previous coatings and oils. Apply Ease Release® 200 using aerosol spray or spray equipment for bulk grades. Hold the can (or spray gun) 6 to 8 inches from the mold surface to ensure a light, even coating. When the molds are new or have been blasted with an abrasive, “season” the mold by applying a heavy coating of release. Heat the mold to process temperature, then wipe the excess with a rag and reapply a light coating of Ease Release® 200 before a regular molding. Ease Release® 200 is fast drying and requires no baking during the normal molding process. Reapply a light coating before each molding.
Finishing - Thorough cleaning of molded parts is required prior to staining, painting, or bonding.