Alja-Safe™ Breeze

 Alja-Safe™ Breeze

没有粉末 - 没有灰尘!
Alja-Safe™Breeze(专利申请中)为新型液体海藻酸盐,与水易于混合,制作独特、安全的模具制造材料。Alja-Safe™Breeze非常适合制作手、脚和其他身体部位的一次性浇注模具。捕捉精细的细节,准确复制原始模型。如果制作身体垂直表面的模具,使用原Alja-Safe™或Alja-Safe™Acrobat™。

特征

Alja-Safe™Breeze易于使用且可快速固化。复制细节并制作出色的临时模具 - 适用于任何身体部位的一至两个复制品。将石膏、Matrix™NEO™(聚合物改性石膏)、Smooth-Cast™300Q超快聚氨酯树脂或快速固化铂金固化硅胶(如Dragon Skin™FX Pro)注入模具中进行复制。
 
要制作任何身体部位可重复使用的模具,请使用Body Double™硅胶。
 
重要提示:本产品尚未经过测试,不应用于牙科应用。


说明

Preparation - Store and use Alja-Safe™ Breeze at room temperature. Alja-Safe™ Breeze may get warm in storage/shipping during the summer months which will cause the material to set too fast. To remedy, store Alja-Safe™ Breeze in a cool area (60°F - 70°F or 15°C - 21°C) for 24 hours before using. Alja-Safe™ Breeze has a limited shelf life and should be used as soon as possible. Do not allow moisture to come into contact with unused Alja-Safe™ Breeze.
 

Shake well before using.

Practice: Make a mold of your thumb – make a mold of something small before going on to larger models. You’ll gain a lot of experience with a small test.

Applying A Release Agent – Alja-Safe™ Breeze will not stick to most surfaces. When making a mold of a body part with body hair, a release preparation is recommended to prevent mechanical lock to the hair. CHOLESTEROL Brand Hair Conditioner (available at most pharmacies) can be applied to hair-covered areas prior to applying Alja-Safe™ Breeze. It can be washed out of the hair easily after use.

Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.


Measuring – Alja-Safe™ Breeze is mixed 5 parts water to 1 part Alja-Safe™ Breeze by volume (5 cups + 1 cup, for example). You can vary the water level somewhat to change consistency of the mixture. Less water will make Alja-Safe™ Breeze slightly thicker. More water will make the mixture thinner. Be careful - too much water may result in the mixture not curing.

Water Quality – Water that has a high mineral content (calcium, phosphate, etc.) may cause any alginate to become “lumpy” or not set properly. A small-scale test is recommended prior to mixing large amounts.

Temperature Of The Water - At 80° F / 27° C, Alja-Safe™ Breeze will have a working time of 3 minutes and a demold time of 8 minutes. Warmer water will cause the material to cure faster (less working time). Colder water will give a longer working time and slower demold time. For best results, pour Alja-Safe™ Breeze into water and mix as directed.


Mixing – Alja-Safe™ Breeze can be hand mixed using a flat, stiff mixing stick with defined edges, but best results will be obtained using a power drill with a mixer attachment. Attach a Jiffy Mixer or Turbine Mixer to a power drill and mix for one minute (depending on volume) to a gel-like consistency. Scrape the sides and bottom of your container using a mixing stick several times.

Color Change Indicator - After mixing for the appropriate amount of time, the color turns from dark blue to light blue and the consistency becomes thicker and creamier. This is your indication that the material is well mixed and ready to be used.

Alja-Safe™ Breeze is best used when poured around an object.

Pouring Around An Object - Once mixed, Alja-Safe™ Breeze can be poured around the hand, foot, fingers or other model in a fixed position inside a container. Suspend the model just above the bottom of the container and have at least ½” (1.27 cm) space between the model and the side walls of the container.

For Best Results: Apply a thin coating of mixed Alja-Safe™ Breeze to the surface of the model by smoothing a small amount of material on by hand. Pour Alja-Safe™ Breeze into the container at the lowest point and let the material rise around the model. Make sure your model has a good clearance distance from the bottom and sides of the container. Keep your model still until the Alja-Safe™ Breeze sets up. You will know the Alja-Safe™ Breeze has set when it is firm and no longer gel-like.


Casting Into The Mold - All alginate molds will deteriorate quickly. It is recommended that you cast into the mold within 4 hours following demold. Materials commonly cast into alginates include Matrix NEO (polymer modified gypsum, available from Smooth-On), plaster, wax, clay and very fast urethane resins (such as Smooth-Cast 300Q). For Soft “Skin-Like” Castings – You can cast Dragon Skin 10 FAST soft silicone rubber into Alja-Safe™ Breeze molds to make realistic hands, limbs, etc.