UreCoat®

UreCoat®是双组分聚氨酯(A +B),混合后刷涂到各种表面上,提供柔软、坚韧和抗冲击的聚氨酯涂层。重量混合比为100A:10B(需要克量级秤),操作时间为8分钟,重涂时间为30分钟,指干时间为2小时,并且在73°F / 23°C下完全固化需16小时。UreCoat®不含邻苯二甲酸盐或VOC。

特征


说明

Amount to Mix and Apply at One Time - Because this is a coating, a small amount goes a long way. Mix only what you can comfortably brush on to your target surface in 8 minutes before material sets up.
 

Measuring and Mixing - Before you begin, pre-mix Part B thoroughly to re-disperse components that may have settled. A gram scale is required to accurately measure 100 Parts A to 10 Parts B. After dispensing into a mixing container, mix thoroughly for 2 - 3 minutes using a square edged mixing stick. Aggressively scrape the sides and bottom of the mixing container several times. Use the square edge of the stick to bring material off of the sides of the container and blend.

Extending Working Time - Reduce the mass of the mixture to increase working time. Example: layer two sheets of aluminum foil together and create a single-use flat tray with vertical sides to contain the liquid. After mixing parts A and B, pour mixture into the aluminum foil to reduce the mass. Your working time will be significantly increased. Applying - Apply a thin layer to the surface, making sure there are no brush strokes. Wait 30 minutes for material to partially cure and apply a second layer. Subsequent layers can be added as desired.

Thinning - To thin UreCoat®, the recommended mix ratio is 100 Parts A + 10 Parts B + 25 or more Parts of mineral spirits depending on the application. Pre-mix solvent into Part A before adding Part B. Observe all safety precautions when handling solvents. Mix thoroughly to a uniform color (no streaks). Spraying UreCoat® is not recommended.

Thickening - UreCoat® can be thickened to a paste-like consistency for brushing or troweling onto surfaces. Ure-Fil® 11 is an effective filler for thickening this material. The recommended maximum filler load when using Ure-Fil® 11 is 100 parts UreCoat® Part A to 10 parts UreCoat® Part B to 15 parts filler by weight. Ensure filler is dry, and pre-mix filler with Part A before combining with Part B.

Surface Finish - UreCoat® will cure with a high gloss surface finish. If a matte surface finish is desired, we have two recommended techniques; once UreCoat® gels or partially cures (30 – 60 minutes after applying), lightly wipe surface with a lint-free cloth that will not shed fibers or a lightly brush surface with a soft paint brush. Do not wait until material is fully cured. Another option is to lightly dust the surface of partially cured UreCoat® with powdered sugar. Once UreCoat® is fully cured, the powdered sugar can be washed away with water, leaving a matte surface finish.

Curing - Allow UreCoat® to cure overnight (at least 16 hours) at room temperature (73°F/23°C) before handling. Full cure time can be reduced heating the material 150°F/60°C for 4 hours. Allow UreCoat® to come to room temperature before handling. Clean Up - Gently scrape as much uncured material from surface as possible with flat edge tool. Remove remaining uncured UreCoat® with alcohol.

介绍产品制作工艺的文章

使用浇注聚氨酯发泡如何制作定制发泡座椅

使用浇注聚氨酯发泡如何制作定制发泡座椅

浇注聚氨酯发泡材料用于制作独特的定制家具作品

› 查看介绍文章

使用UreCoat制作不可毁坏的道具

使用UreCoat制作不可毁坏的道具

视频演示如何使用雕刻软发泡和UreCoat聚氨酯涂层料制作仿真发泡道具岩石

› 查看介绍文章

使用UreCoat制作神奇女侠Cosplay

使用UreCoat制作神奇女侠Cosplay

如何使用泡沫纸和Smooth-On的UreCoat制作服装铠甲

› 查看介绍文章

使用UreCoat涂层制作自己的橡胶柄

使用UreCoat涂层制作自己的橡胶柄

视频演示如何使用UreCoat涂覆工具手柄。涂覆后的手柄容易握持并且使用安全

› 查看介绍文章

使用UreCoat制作仿真藤

使用UreCoat制作仿真藤

视频演示如何制作特别耐用和耐动物仿真藤

› 查看介绍文章