NOVOCS™ Gloss

NOVOCS™溶剂为可以快速蒸发的低粘度有机硅溶剂。NOVOCS™在稀释PsychoPaint®涂层硅胶非常有效,可通过刷子或喷枪将其涂布到固化的铂金固化硅胶道具和假体上。当用作稀释硅胶稀释剂或涂层硅胶的溶剂时,NOVOCS™ Gloss具有光泽。

警告 - 易燃液体和蒸气。远离火源并遵守处理易燃物品的注意事项。

特征


说明

Materials should be stored and used in a warm environment (73°F / 23°C). This material has a limited shelf life and should be used as soon as possible. Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk.
 

Mix the A and B components of two component silicone sytems before adding NOVOCS™. Add the desired proportion of NOVOCS™ solvent to create a thinner silicone mixture which can be brushed or airbrushed onto the surface of a cured silicone casting.

Example Recommended Ratios For Use:

Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.

介绍产品制作工艺的文章

使用NOVOCS有机硅溶剂收缩浇注件

使用NOVOCS有机硅溶剂收缩浇注件

使用者可以在有机硅中混合18%-22%的NOVOCS有机硅溶剂收缩硅胶模具