Plasti-Paste® II

Plasti-Paste® II

新型Plasti-Paste®II为双组分纤维填充树脂,专为垂直表面应用而设计。无味配方、原有的Plasti-Paste®配方的改进版本,固化后产品在以下方面有所不同:
1. Plasti-Paste II不含邻苯二甲酸酯。
2. 固化后树脂可以涂漆(原PlastiPaste®不能)
3. 它具有更好的耐热性,更坚硬,刚性更高。
 
A组分为液体,B组分为膏状物。体积混合比例为1A:2B(62A:100B重量比)。取决于质量,室温下操作为10分钟。取决于质量。室温下的固化可使用时间约为90分钟。室温下,24小时完全固化。通过加热可以加速固化时间。
 
混合材料可以保持在垂直表面,不下垂,并且固化成坚固、耐用和轻质的树脂。可以使用Smooth On的So-Strong®颜色着色。树脂可用于创造主题环境或特殊效果,用作“母模”材料以加强橡胶模具和各种其他应用。树脂也是一款强大的粘合剂,可用作各种工业应用的修补材料。固化后的树脂可以打磨、机械加工并涂丙烯酸瓷漆。

特征

说明

Preparation – Materials should be stored and used in at room temperature (73° F / 23° C). This product has a limited shelf life and should be used as soon as possible. Mixing should be done in a well-ventilated area. Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk. If making a 2 or more piece mother mold, apply appropriate shim apparatus to rubber mold exterior.
 

Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.

Applying A Release Agent – This product is adhesive and will bond to many surfaces. A sealer followed by a release agent is necessary to facilitate demolding when applying as a mother mold over a cured mold rubber. Use Sonite® Wax followed by a coating of Universal® Mold Release or Ease Release 200 release agent. A liberal coat of release agent should be applied onto all surfaces that will contact the plastic. You can also apply aluminum foil as a barrier over the surface followed by an application of Mold Release agent.

PRE-MIX Part B Before You Start – Part B is a thick paste containing oil that needs to be pre-mixed before being dispensed into measuring container. Dig deep to re-disperse oil & paste components that may have separated.

Measuring – The components of Plasti-Paste® II requires two different sized containers. The first will be used for measuring out amounts of Part A and Part B. The second should be large enough to contain both components and allow thorough mixing. IMPORTANT: Shelf life of Part A (Yellow Container) is reduced after opening. Remaining product should be used as soon as possible. XTEND-IT® Dry Gas Blanket will prolong shelf life of unused liquid urethanes.

Mixing – Mix Ratio is 1A:2B by volume (62A:100B by weight). (Step 1) Fill measuring container to the top with Part B paste, making sure to eliminate any air voids. Level off the top of the container and remove any excess material. The paste should then be thoroughly emptied into a larger container that will act as your mixing container. Repeat As Necessary. (Step 2) Fill the measuring container to the top with Part A liquid and empty into mixing container. Mix thoroughly for 2-3 minutes making sure that you scrape the sides and bottom of the mixing container several times. Eliminate color streaks. If adding So-Strong® color tints, pre-mix color with the Part B before adding Part A.

Mixing Large Batches - A ‘Turbine’ mechanical mixer attached to a power drill will make mixing large batches of material much easier.


IMPORTANT: Shelf life of product is reduced after opening. Remaining product should be used as soon as possible. Immediately replacing the lids on both containers after dispensing product will help prolong the shelf life of the unused product. XTEND-IT® Dry Gas Blanket (available from Smooth-On) will significantly prolong the shelf life of unused liquid urethane products.


Applying – Mixed material thickens quickly and pot life is limited. Do not delay between mixing and applying. To increase working time, spread entire container contents over rubber mold surface and cover and spread mixture to uncovered areas. Apply uniformly with spatula over mold surface. Material will adhere to itself if additional layers are needed. Apply at least 3/8” (1 cm) thickness, making sure rubber mold is thoroughly covered. For maximum strength and heat resistance, ½” (1.27 cm) thickness is recommended. Large molds may require added thickness for support shell stability. Supports (wood or metal) may be embedded for added stability and handling. Prevent a jagged surface; Final layer of Plasti-Paste® II can be smoothed by wiping solvent (denatured alcohol or acetone) onto surface with gloved hand.

Making A Two Piece Shell – Plasti-Paste® II will bond to most surfaces and itself tenaciously. A barrier coat of paste wax followed by Universal® Mold Release applied to all surfaces is necessary to prevent adhesion. Applying aluminum foil to the contours of all surfaces followed by Universal® Mold Release will also prevent adhesion.

If You Want To Paint Cured Plastic – For best results, measure 62 Parts A + 100 Parts B by weight using a gram scale.

Curing – Plastic will be hot immediately following cure. Let cool to room temperature before handling. Material will develop handling strength and can be handled in about 90 minutes depending on mass. At this point, it is stable enough to demold, re-assemble over rubber mold and make a casting (hold 2 or more piece assemblies together with elastic bands, mold straps or bolts). Large sections should be bolted together to minimize distortion. Full strength develops in 24 hours.

Heat Resistance – Fully cured plastic with a minimum thickness of ½” (1.27 cm) will resist temperatures up to 130°F/55°C. To improve heat resistance to 158°F / 70°C, post cure material at 150°F/65°C for 16 hours.

If machining or sanding cured plastic, wear NIOSH approved mask to prevent inhalation of residual particles.


Painting – Make sure surface is clean and free of release agents or other contaminants. Cured plastic can be painted and/or primed and then painted with acrylic enamel paints. Let paint fully dry before putting part into service.

Storage – For best storage results, cast into rubber mold with a gypsum plaster or other dimensionally stable material, assemble mold inside the Plasti-Paste® II support shell and store assembled molds on a level surface indoors at room temperature in a dry place.

介绍产品制作工艺的文章

混凝土仿石手盆的制作

混凝土仿石手盆的制作

使用Rebound25涂刷型硅胶,制作仿石手盆模具

› 查看介绍文章

修复普林斯顿大学历史历史性混凝土标志

修复普林斯顿大学历史历史性混凝土标志

来自Paolini Cast Stone的John Paolini修复历史性混凝土标志

› 查看介绍文章

3D空腔模型涂刷型模具制作

3D空腔模型涂刷型模具制作

展示使用Smooth-On的Rebound25硅胶如何制作美洲狮头模具

› 查看介绍文章

制作聚氨酯树脂化妆假体模具

制作聚氨酯树脂化妆假体模具

概述模具的结构,浇注F X硅胶化妆器具

› 查看介绍文章

使用Rebound25修复建筑托臂

使用Rebound25修复建筑托臂

如何制作托臂模具用于纽约布鲁克林建筑修复项目

› 查看介绍文章