Ignite®

Ignite®

IGNITE®液体荧光颜色与Smooth-On的聚氨酯橡胶、聚氨酯塑料,聚氨酯发泡(硬泡和软泡)、硅胶兼容。在紫外线或“黑光”下荧光或“发光”效果最佳。当Ignite颜色与透明或半透明聚氨酯橡胶(如Clear Flex 50)或塑料(如Smooth-Cast325)一起使用时,可以实现最显着的色彩效果。
 
Ignite®9色包装为9色体验包装。
 
什么使使用Ignite®颜料的浇注件看起来会发光?当将Ignite荧光颜色添加到聚氨酯材料中时,与使用SO Strong®颜色制作的浇注件对比,眼睛可以看见更多来自固化材料中紫外光线。环境光线中的浇注件看起来更亮,并且在紫外线下会发光。

特征

说明

To get you started, we offer the following colorant loading levels. Results may vary.
 

By Weight Using A Gram Scale: Add Ignite® colorant at a ratio of between 0.5% - 1.5% of the total weight (Parts A + B mixed) of the material being cast. 1% pigment yields the best results. Adding more than 1.5% by weight offers no benefit and is a waste of the colorant. Too much colorant may cause cure inhibition.

By Volume Measured In Drops: Add 30 drops of Ignite™ per 3 oz (88 ml) of mixed urethane material. If using a translucent material (like Smooth-Cast 325) you can use 15 drops to maintain translucency of the material.

Pre-Mix Before Using: Ignite® colorants are pigment dispersions and may separate over time. They must be thoroughly pre-mixed in the container before using with a liquid urethane product.

Directions For Use: After dispensing the required amount of urethane material Parts A and B into measuring containers, add colorant to Part B and mix thoroughly. Combine Parts A and B into a mixing container and mix as directed by the urethane product technical bulletin. Blending Colors - You can combine different colors on a pallete to create a custom color before adding to liquid urethane product as directed above.

There are no issues when using this product with urethane rubbers, plastics and foams or tin-catalyzed silicones. However…Ignite® pigments will drastically thicken platinum silicone rubber. Adding Ignite® colorants to a Smooth-On platinum cure silicone such as Dragon Skin® will make the silicone notably thicker, thereby affecting its ability to be vacuum degassed. Recommended loading maximum is 1% Ignite pigment by weight. An option for using Ignite® colorants with a platinum silicone may be to use pigmented material as paint for brushing on to an existing platinum silicone casting or appliance. You can use Ignite® colorants with our Psycho Paint® system.

Smooth-On offers this color guide as a general reference only and assumes no responsibility for color accuracy or matching. Results will vary from one material to another. The end user is solely responsible for determining color suitability and accuracy. Small scale testing is recommended. User determines amount to add;If this is your first time adding color tint or pigment to a urethane, epoxy or silicone system, you may want to test the color effect by adding a few drops to a small amount of urethane material and observe the outcome. It may take a few test castings to attain the desired color outcome.

Looking for a clear fluorescent additive? Cryptolyte® is a clear additive that can be added to urethane or silicone materials that will cause cured material to glow a bright blue when exposed to UV light (black light).