Form™AIR HT为低密度、轻质环氧腻子,在室温固化时可耐300°F /149°C,加热后固化可达400°F / 204°C。产品为低气味、低收缩配方,易于使用。FreeForm™AIR HT按体积或重量混合比2A:1B用手混合。具有很长的工作时间,并在室温下过夜固化成坚硬、刚性环氧树脂。环氧树脂非常坚固,具有模型板的特性。可以打磨、成型、钻孔、攻丝和CNC加工/打磨。
环氧层压 - 层压Free Form™AIR HT腻子在EpoxAmite™HT层压环氧树脂和玻璃纤维布、碳纤维或其他纤维之间,制作轻质复合材料部件。不需要用液体环氧树脂进行多层层压; 节省时间和人力。
环氧工具具应用 - 用作切片材料。也适用于夹具和固定结构。
用作轻质粘合剂,FreeForm™AIR HT可粘合自身和各种表面,包括木材、石材和EpoxAcoat™HT表面涂层环氧树脂。
操作时间/工作时间 - 此材料对质量敏感。一次混合的材料越多,使用的时间就越少。工作提示; 如果大量混合,用擀面杖压扁腻子,以减少质量浓度,延长操作时间。
PROCESSING RECOMMENDATIONS
Safety – Use in a well-ventilated area (“room size” ventilation). Generally, if you use any epoxy system on a regular basis, wearing a NIOSH approved respirator is advised. Wear safety glasses, long sleeves and rubber gloves to minimize skin contact. Wear nitrile or vinyl gloves only.
Preparation – Materials should be stored and used at room temperature (73°F/23°C). This product has a limited shelf life and should be used as soon as possible. Mixing should be done in a well-ventilated area. Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk. If making a 2 or more piece mother mold, apply appropriate shim apparatus to rubber mold exterior. Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.
Applying A Release Agent – For releasing epoxy from nonporous surfaces such as resin, metal, glass etc., use Ease Release™ 200 or 205 (available from Smooth-On) to prevent adhesion.
This product is mixed by hand. You must wear gloves when mixing this material, wearing vinyl gloves reduces inhibition risk.
MEASURING
Free Form™ AIR HT putty comes as two parts. Dispense 2A:1B by weight or volume. These products have a limited shelf life and should be used as soon as possible.
MIXING
Knead parts together aggressively to a uniform color and apply quickly to surface of tool or mold.
APPLYING & LAMINATING
Applying – Mixed Free Form™ AIR HT is a dough that can be applied up to 1.5” (3.81 cm) thickness. Mix only enough material to be used at one time. Free Form™ AIR HT will bond to itself.
Laminating - Free Form™ AIR HT can be used in conjunction with EpoxAcoat™ HT surface coat and EpoxAmite™ HT laminating resin to create a strong and lightweight composite tool or mold. Free Form™ AIR HT can also be used to stabilize tools during the heat post curing process to help reduce deformation.
CURING & HEAT RESISTANCE
Cure Time - Refer to specified Cure Times in the Product Overview section at room temperature depending on mass. Cured material will be hard and unable to penetrate with a finger nail. Cured epoxy can now be dry sanded. If machining or sanding, wear NIOSH approved mask to prevent inhalation of particles. Pot Life and Cure Time values are dependent on mass and mold configuration, as epoxies are mass-sensitive.
Heat Resistance – Putty cured at room with a minimum thickness of ½” (1.27 cm) will resist temperatures up to 300°F/149°C
Post Curing For Maximum Heat Resistance - The tool should be allowed to cure at room temperature (73°F/23°C) for 16 hrs. At that point, preheat oven to 200°F and apply the following oven cure. Cycle should be 50 degrees per hour (tool temperature, not air temperature).
1 Hour at 200°F/93°C , 1 Hour at 250°F/121°C, 1 Hour at 300°F/149°C, 1 Hour at 350°F/ 177°C, 1 Hour at 400°F/204°C, then turn off oven and allow tool to cool to room temperature.
This post cure schedule will result in a heat resistance of 400°F/204°C.
Removing Uncured Free Form™ AIR HT Epoxy Putty - Remove as much uncured material from the surface as possible. Clean any residue with soap and water. Optional - Use E-POX-EE KLEENER™ available from Smooth-On.