Alja-Safe™ Acrobat

 Alja-Safe™ Acrobat

Acrobat™为原Alja-Safe™人体浇注海藻酸盐的纤维增强“非下垂”版本。Acrobat更稠,并且可以附着在垂直表面。用户可以更好地控制面部、躯干等部位的模型制作。Acrobat™可以从所有身体表面复制完美细节,并且适用于制作临时模具,用于制作浇注蜡、石膏、Matrix™NEO™(聚合物改性石膏)、铂固化硅胶或Smooth-Cast™300Q超快聚氨酯树脂的高度精细复制品。

特征

易于使用 - 混合比例为1份Alja-Safe™Acrobat™粉末:1份水(体积比1:1)。假设水温为80°F /27°C,工作时间为5分钟,固化时间为8分钟。
 
与原Alja-Safe™一样,Acrobat™皮肤安全,不含结晶二氧化硅(一种已知的致癌物质)。
 
要制作任何身体部位可重复使用的模具,请使用Body Double™硅胶。
 
重要提示:本产品尚未经过测试,不应用于牙科应用


说明

Preparation - Store and use Alja-Safe™ Acrobat™ in a dry environment at room temperature. Alja-Safe™ Acrobat™ powder may get warm in storage/shipping during the summer months which will cause the powder/water mixture to set too fast. To remedy, store Alja-Safe™ Acrobat™ in a cool area (60°F - 70°F or 15°C - 31°C) for 24 hours before using. Alja-Safe™ Acrobat™ has a limited shelf life and should be used as soon as possible. Do not allow moisture to come into contact with unused Alja-Safe™ Acrobat™. Use only with adequate ventilation.
 

Practice: Make a mold of the back of your hand – make a mold of something small before going on to larger models. You’ll gain a lot of experience with a small test.

Applying A Release Agent – Alja-Safe™ Acrobat™ will not stick to most surfaces. When making a mold of the head, a release preparation is recommended to prevent mechanical lock to the hair. Cholesterol based hair conditioner (available at most pharmacies) can be applied to hair-covered areas prior to applying Alja-Safe™ Acrobat™. It can be washed out of the hair easily after use.

Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.


Measuring – Alja-Safe™ Acrobat™ is mixed 1 part water to 1 part powder by volume (1 cup + 1 cup, for example). IMPORTANT - You must pack the powder firmly into the measuring cup. You can vary the water level somewhat to change consistency of the mixture. Less water will make Alja-Safe™ Acrobat™ thicker. More water will make the mixture thinner. Be careful…too much water will may result in the mixture not curing.

Water Quality – Water that has a high mineral content (calcium, phosphate, etc.) may cause any alginate to become "lumpy" or not set properly. A small-scale test is recommended prior to mixing large amounts.

Temperature Of The Water - At 80° F / 27° C, Alja-Safe™ Acrobat™ will have a working time of 8 minutes and a demold time of 10 minutes. Warmer water will cause the material to cure faster (less working time). Colder water will give a longer working time and slower demold time. For best results, sift Alja-Safe™ powder into water and mix as directed.


Mixing – Alja-Safe™ Acrobat™ can be hand mixed, but best results will be obtained using a power drill with a mixer attachment. Attach a Jiffy Mixer or Turbine Mixer to a power drill and mix for one minute (depending on volume) to a gel-like consistency – smooth without any powder lumps. Jiffy mixers are available at many hardware stores. Turbine Mixers will yield the best mix and are available from Smooth-On or your Smooth-On distributor.

Alja-Safe™ Acrobat™ is designed to be applied to vertical surfaces.

For Best Results: Wet the surface of the model’s skin before applying. Apply a thin coating of Alja-Safe™ Acrobat™ to the surface of the model by brushing, smoothing the material on by hand or using a plastic spatula. Keep your model still until the Alja-Safe™ Acrobat™ sets up. You will know the Alja-Safe™ Acrobat™ has set when it is firm and no longer gel-like.

You may want to experiment with the amount of water added to Alja-Safe™ Acrobat™ to find a thicker consistency that is right for vertical surface application. For example, some customers mix 1 part water to 1.5 parts Alja-Safe™ Acrobat™.

Applying A Support Shell - Once the material cures, a support shell will be necessary to support the Alja-Safe™ Acrobat™ mold. Gypsona brand medical grade plaster bandages are ideal for this purpose, and are available from Smooth-On or your Smooth-On distributor.


Casting Into The Mold - All alginate molds will deteriorate quickly. It is recommended that you cast into the mold within 4 hours following demold. Materials commonly cast into alginates include Matrix NEO (polymer modified gypsum, available from Smooth-On), plaster, wax, clay and very fast urethane resins (such as Smooth-Cast™ 300Q). For Soft "Skin-Like" Castings – You can cast Dragon Skin™ FX Pro™ soft silicone rubber into Alja-Safe™ Acrobat™molds to make realistic hands, limbs, etc.

介绍产品制作工艺的文章

用Alja-Safe Acrobat制作面模

用Alja-Safe Acrobat制作面模

Ajia-Safe Acrobat 为原Alja-Safe alginate纤维填充“不下垂”版本。

› 查看介绍文章