Spray-Up: Spray-Up GFRC refers to the process of using a spray pump, either rotor/stator or peristaltic, to spray a GFRC slurry and continuous strand AR glass fiber roving.  It uses a specialized spray gun with an integrated fiber chopper.  The GFRC slurry and fiber are fed to the gun separately and the chopper cuts the fiber and introduces it into the slurry stream at the spray nozzle.  Spray-Up typically contains a minimum of 4% glass fiber.  In the US and several international markets, Spray-Up GFRC “skins” are panelized on a steel stud frame and weigh 20-25 lbs per square foot.

Premix:  Premix GFRC incorporates AR glass fibers, or chopped strands, into the slurry during mixing and slurry preparation.  The Premix process is further broken down into various production techniques such as spray premix, cast premix, pultrusion and hand lay-up.  Premix is most often used for smaller GFRC parts and rarely incorporates a frame.  Without the frame, GFRC will weigh 7-10 lbs per square foot.

免责声明
这些FAQ文章作为参考,并提供模具制造和浇注过程中遇到问题的可能解决方案。由最终用户确定任何特定应用的适用性。我们不做保证。使用任何材料前参考所提供的技术公告(TB)和安全数据表(SDS)。在大范围使用前,建议小范围试验确定任何建议的适用性。