Smooth‑Sil™ 933 阻燃铂金硅胶

Smooth‑Sil™ 933 阻燃铂金硅胶

Smooth-Sil 933阻燃型铂金硅胶
注:产品包装可能有所不同

Smooth-Sil 933阻燃型铂金硅胶专为阻燃垫片和灌封应用而设计。

Smooth-Sil 933阻燃型铂金硅胶是一款邵氏硬度 33A 的铂金硅胶,按体积或重量 1A:1B 混合。硅胶在室温(73°F/23°C)下固化,收缩率极低。建议进行真空脱气处理,以最大程度减少固化后硅胶中的气泡。固化后的材料通过 UL 94 V-0 认证。

Smooth-Sil 933可在6小时内固化为柔软、坚固且抗撕裂的硅胶,长期收缩率极低。通过添加Silc Pig硅胶颜料,可实现无数种颜色效果。应用包括阻燃外壳的电气灌封、医疗设备和电器的垫片制作,以及其他需要阻燃、柔性硅胶密封的应用场合。

注意:即使表面封闭,本产品也不会在含硫表面固化。

特征

  1. 阻燃等级达 UL 94 V-0
  2. 高性能垫片和灌封硅橡胶

说明

PREPARATION...Safety – Use in a properly ventilated area (“room size” ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk. Wear vinyl gloves only. Latex gloves will inhibit the cure of the rubber.

Store and use material at room temperature (73°F/23°C). Warmer temperatures will drastically reduce working time and cure time. Storing material at warmer temperatures will also reduce the usable shelf life of unused material. These products have a limited shelf life and should be used as soon as possible.

Cure Inhibition – Addition-cure silicone rubber may be inhibited by certain contaminants in or on the pattern to be molded resulting in tackiness at the pattern interface or a total lack of cure throughout the mold. Latex, tin-cure silicone, sulfur clays, certain wood surfaces, newly cast polyester, epoxy or urethane rubber my cause inhibition. If compatibility between the rubber and the surface is a concern, a small-scale test is recommended. Apply a small amount of rubber onto a non-critical area of the pattern. Inhibition has occurred if the rubber is gummy or uncured after the recommended cure time has passed.

Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.

Even with a sealer, Smooth-Sil™ 933 will not cure against surfaces containing sulfur. If you are not sure if your clay contains sulfur, do a small compatibility test before using for an important project.

Applying A Release Agent - Although not usually necessary, a release agent will make demolding easier when pouring into or over most surfaces. Ease Release™ 200 is a proven release agent for making molds with silicone rubber. Mann Ease Release™ products are available from Smooth-On or your Smooth-On distributor.

IMPORTANT: To ensure thorough coverage, lightly brush the release agent with a soft brush over all surfaces of the model. Follow with a light mist coating and let the release agent dry for 30 minutes.

If there is any question about the effectiveness of a sealer/release agent combination, a small-scale test should be made on an identical surface for trial.


MEASURING & MIXING...Before you begin, pre-mix Part A and Part B separately. After dispensing required amounts of Parts A and B into mixing container (1A:1B by volume or weight), mix thoroughly making sure that you scrape the sides and bottom of the mixing container several times.

After mixing parts A and B, vacuum degassing is recommended to eliminate any entrapped air in liquid rubber. Your vacuum pump must pull a minimum of 29 inches of mercury (or 1 Bar / 100 KPa). Leave enough room in container for material expansion. Vacuum material until it rises, breaks and falls. Vacuum for 1 minute after material falls


POURING, CURING & MOLD PERFORMANCE...
For best results, pour your mixture in a single spot at the lowest point of the containment field. Let the rubber seek its level up and over the model. A uniform flow will help minimize entrapped air. The liquid rubber should level off at least 1/2” (1.3 cm) over the highest point of the model surface.

Curing / Post Curing - Allow rubber to cure for 6 hours at room temperature (73°F/23°C) before demolding. Heat Curing - Time to demold can be reduced with mild heat. Example: After pouring Smooth-Sil™ 933 at room temperature, place the mold in a hot box or industrial oven at 150°F (60°C). This may reduce the demold time substantially. Note - time will vary depending on mold thickness.