Silc Pig™ 电荧光有机硅颜料用于锡固化硅胶,如Mold Max™ 半透明“T”系列产品和铂金固化硅胶,如Dragon Skin™ 和 Ecoflex™硅胶着色。Silc Pig™ 电荧光颜料还可以与 Smooth-On的皮肤特效系统配合使用,例如Psycho Paint™ 和 Skin Tite™。荧光或“发光”效果在紫外线或“黑光”下最大化。当 Silc Pig™ 电荧光颜料与透明或半透明有机硅一起使用时,可实现最引人注目的色彩效果。
什么使用 Silc Pig™ 电荧光颜料制成的浇注件看起来会发光?
当将 Silc Pig™ 电荧光颜料添加到有机硅中时,与使用标准 Silc-Pig™颜料制成的浇注件相比,眼睛可以看到更多来自固化材料的紫外线。浇注件在环境光下显得更亮,在紫外线(黑光)下看起来更亮。
Instructions
Custom colors are possible by blending different Silc Pig™ Electric Fluorescent Pigment colors. Attaining just the right color for your application may require trial and error testing. Small scale testing is recommended before using substantial amounts of material for any project.
Silc Pig™ Electric Fluorescent pigments are concentrated, so a little goes a long way when coloring Smooth-On silicone products. Recommended loading range is .001% to 3% of total silicone system weight. Do not overload silicone rubber with Silc Pig™ Fluorescent or cure inhibition may occur. Pre-mix Silc Pig™ Electric Fluorescent pigment in container thoroughly before dispensing as settling may have occurred. Add Silc Pig™ Electric Fluorescent pigment to the Part A side of the silicone rubber system and mix well before adding Part B.
For directions on using Dragon Skin™ or other Smooth-On silicone rubbers, consult the technical bulletin for that product.