Vertical Mix™

Vertical Mix™

Buddy Rhodes Vertical Mix™是一种易于使用的水泥基铺面层,混合容易并应用于垂直表面雕刻、雕塑或压印各种纹理。产品轻巧、零坍落度配方,可用于创建主题环境、动物园和水族馆展示,装饰板和公共雕塑。配合Buddy Rhodes广泛的颜料产品,实现无限的色彩。Buddy Rhodes Glazes也可以应用于固化混凝土,以实现多种颜色效果。Buddy Rhodes提供唯一经过测试和认证的E-84 A级阻燃性的立面混合材料。

重要提示:必须将RAMP™粘合剂和固化促进剂与Buddy Rhodes Vertical Mix™一起使用。

特征

说明

Surface Preparation - Vertical Mix can be applied to a variety of surfaces, provided the surface is clean and stable. Any loose material should be repaired or removed prior to surface preparation. Priming Surfaces with Buddy Rhodes RAMP: Buddy Rhodes RAMPTM is an economical bonding primer and cure promoter. Add 100 parts of clean water to 100 parts RAMP (50/50) into a spray bottle, pump sprayer, or similar. Shake vigorously. Spray an even, thin coating of primer on all surfaces and allow to become tacky (partially dry, sticky to the touch) before applying Vertical Mix. If primer dries completely, reapply and wait until tacky before proceeding

Preparation - Getting Ready to Mix Have all ingredients assembled before you start. Wear vinyl or nitrile gloves, protective eye wear and a dust mask. Use an accurate scale for weighing components. Use materials between 50°F and 90°F (10°C - 32°C). Colder temperatures will slow the reaction and warmer temperatures will accelerate it. Preparations should be made to ensure that the applied material is not exposed to rain or temperatures below 50°F/10°C for the first 48 hours. The temperature of the Vertical Mix is also important and will affect the outcome. Once the temperature of the mix reaches 70°F/21°C, the reaction begins to accelerate. Using a laser thermometer to monitor, keeping the temperature of the mix near 60° F/15° C. In warm environments, substitute up to 50% by weight of the water with ice. Vertical Mix has a shelf life of 1 year after purchase if kept in a dry, moisture free environment. Once opened, the material should be used as soon as possible.

Recipe For Buddy Rhodes Vertical Mix

Buddy Rhodes Vertical Mix Buddy Rhodes RAMP Water
By Weight 34 lb (15.4 kg) 3 lb (1.36 kg) 7.5 lb (3.4 kg)
By Weight [100 Parts] [8.82 Parts] [22.06 Parts]
By Volume 1 Bag of Vertical Mix 42 fluid oz. (1.24 l) 115 fluid oz (3.4 l)

Mixing Instructions - Use clean, potable water and clean mixing vessels. Use a handheld mortar mixer to blend. If mixing on a regular basis or for a large project, investing in a larger mortar mixer may be justified. Measuring and Mixing: Combine water and RAMP into a clean mixing container. If you are adding a Buddy Rhodes color pigment, disperse the pigment into the liquid at this time. Slowly add the Vertical Mix into the liquid and blend with a mechanical mixer until homogenous. Use a margin trowel to scrape the sides of the pail to ensure there is no dry, unmixed material remaining. Continue mixing, adding up to 16 fluid oz. (475 ml) of additional water per bag to reach desired consistency. Applying: Spread the blended Vertical Mix onto the chosen surface. Material can be applied by hand, by trowel, or with a mortar sprayer. To ensure the strongest bond it is often best to spread a thin layer onto the surface first, followed immediately by a thicker build. Maintain a minimum thickness of 0.75" (19 mm). Stamping/Texturing: While the mix is in the plastic state, it can be easily stamped with texture mats or rollers. A liquid release should be applied to the mat or roller to avoid sticking of the material. Carving/Sculpting: When used at room temperature (73°F/23°C), Vertical Mix will reach initial set in 1-2 hours (depending on environmental conditions). The material will continue to get firmer as time passes. Various techniques can be used to carve and detail the design using plastic, wood or metal sculpting tools. Note: If the entire mass of the newly applied material moves excessively while tooling, stop and allow for longer cure before proceeding. Post texturing/Coloring: Allow the material to cure for at least 16 hours. Cured Vertical Mix may be topically colored with acid stains or water-based color stains such as Buddy Rhodes Glazes. The most realistic coloring will be achieved with various layers of multiple colors and concentrations. Allow all topical colors to completely dry before applying any concrete sealer.

Sealing - Concrete is an inherently porous material and should be sealed for particular environments and uses. Allow the concrete to cure for at least 7 days before sealing. Choose the sealer that best fits the needs of the finished piece and the skill level of the person applying it. Exposures to excessive sun and water will determine the best sealer suitable for the application.