XTC-3D®

XTC-3D®

XTC-3D用于3D打印件的光滑和饰面保护涂层。双组份混合涂刷到3D打印件表面。涂层自流平并且浸润均匀,无刷痕。操作时间10分钟,固化时间大约4小时(取决于质量和温度)。XTC-3D固化成坚硬、耐冲击涂层,可以打磨、上底漆和上色。添加颜色和金属效果容易。

特征

  1. 使用成本低-1盎司材料可以覆盖100以上平方英寸(2.3m2/kg, 涂层厚度为0.04cm)。
  2. 节省90%时间和劳动力:XTC-3D填充3D打印件条纹中,形成光滑、高光泽表面。几乎无需后期的修饰
  3. 涂覆任何3D打印表面:XTC-3D可以用于SLA和SLS打印件。有效用于PLA、ABS、Laywoo、粉末印刷件和其它坚硬材质上。也可用于涂覆EPS、EPDM和聚氨酯发泡、木材、灰泥、纤维、纸板和纸。
  4. XTC-3D不含VOC’s、邻苯二甲酸酯或磷酸盐

说明

Preparation – Materials should be stored and used in a room temperature environment (73°F/23°C). Elevated temperatures will reduce Pot Life. XTC-3D® Part A resin and Part B Hardener must be properly measured and thoroughly mixed to achieve full, high-strength, solid-cure properties.
 

Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.

Avoid eye and skin contact. Avoid breathing fumes - use in a well ventilated area. NIOSH approved respirator is recommended. Wear safety glasses, long sleeves and rubber gloves to minimize skin contact. This material has a high exotherm (generates heat). Do not mix components in glass or foam containers.

Coverage – A very small amount of XTC-3D® is needed to coat an average size 3D print. 1 oz / 28.3 grams of mixed material will cover 101 in2 (651 cm2 ) applied at 1/64” (.04 cm) thickness.

Pre-Mix Part B: Before using, shake container vigorously.

Measuring and Dispensing – You need to be accurate in measuring for XTC-3D® to cure properly. Parts A and B can be measured by either volume or weight. Dispense proper proportions of parts A and B into clean plastic, metal or wax-free paper containers (do not use foam or glass cups).

Extending Working Time - If left in a mixing cup with a concentrated mass, pot life will be short and material may cure in your cup due to exotherm. Important - Reduce the mass of the mixture to increase working time. Example: layer two sheets of aluminum foil together and create a single-use flat tray with vertical sides to contain the liquid resin. After mixing parts A and B, pour mixture into the aluminum foil to reduce the mass. Your working time will be significantly increased.

Mixing – Be sure mixing utensils have a square edge and are clean. Combine and mix proper amounts of Parts A and B. Mix thoroughly for at least 1 minute. Aggressively scrape the sides and bottom of mixing container several times. Use the square edge of mixing stick to bring material off of the sides and bottom of container and blend.

Important - Mixed XTC-3D® Resin is exothermic, meaning it generates heat. A large, concentrated mass of mixed material in a container can generate enough heat to melt a plastic cup, burn your skin or ignite combustible materials. If material begins to exotherm, move it to an open air environment.

Adding Color - XTC-3D® can be colored with SO Strong® color tints, UVO® color pigments or ignite color pigments. Pre-mix color with Part A before combining with Part B.

Adding Fillers - A variety of dry fillers can be added such as Cast Magic® or bronze or other metal powders, Glow Worm®, Quarry Tone® or Ure-Fil® powders. The maximum filler load is an amount equal to Part A by volume. Pre-mix filler with Part A before combining with Part B.

Applying XTC-3D® - Use a disposable chip brush or foam brush to apply XTC-3D®. To achieve the thinnest coating possible we recommend applying material with a foam brush. Brushing on one thin layer of mixed material is recommended for most prints to create a smooth, uniform coating: less than 1/64“(.039 cm). To avoid drips and runs, continue brushing and working the surface until the resin begins to set up. For particularly complicated prints with intricate detail you may want to coat one a section at a time for better control. XTC-3D® bonds to itself.

If Adding More Layers - allow first layer to partially cure until “tacky hard” before applying the next layer. For best results, each layer should be applied thinly: less than 1/64“(.039 cm).

Curing: One layer will cure tack free in about 2 hours at room temperature (73°F/23°C). Mild heat (150° F/60° C) will cure material within 15 minutes. Be careful: some 3D print media will melt at temperatures above 200°F. Fully cured material will be hard and unable to penetrate with a finger nail.

Post Finishing – Cured material can be machined or sanded (wear NIOSH approved respirator mask to prevent inhalation).

Painting – XTC-3D® can be painted and/or primed and then painted with acrylic enamel paints. For best results, lightly sand surface prior to painting.

Thinning XTC-3D® for Coating Starch / Powder Printed Parts: Viscosity can be lowered with acetone or denatured alcohol to penetrate porous parts.

The more solvent added, the longer XTC-3D® will take to cure. Cured material will be more flexible.

Smoothing Surface – granular surface texture can be smoothed by applying a second coat of XTC-3D® (for glossy finish) or lightly sanding for matte finish.

Warning – Do Not Spray XTC-3D® Read SDS for further information.

Applying a Release Agent – For applications where adhesion is not desired, a spray release Ease Release® 200 available from Smooth-On may be used.

Removing Uncured Material: Scrape as much material as possible from the surface using a scraper. Clean the residue with E-POX-EE KLEENER® available from Smooth-On, lacquer thinner, acetone or alcohol. Follow safety warnings pertaining to solvents and provide adequate ventilation.

介绍产品制作工艺的文章

如何用树脂包裹鲜花

如何用树脂包裹鲜花

Jara使用XTC-3D环氧树脂包裹丝绢花,制作具有长期光泽的展品

› 查看介绍文章

制作耐用传送带清理器

制作耐用传送带清理器

从PLA 3D打印原型,了解如何用工业橡胶制作耐用传送带清理器

› 查看介绍文章

3D打印件快速添加金属饰面效果

3D打印件快速添加金属饰面效果

视频演示使用XTC-3D环氧使3D打印PLA件如何真金属

› 查看介绍文章

使用XTC-3D在3D打印件上添加颜色效果

使用XTC-3D在3D打印件上添加颜色效果

视频演示如何使用XTC-3D环氧涂层使3D打印建筑模型表面光滑并具有颜色

› 查看介绍文章