使用EZ-Spray 有机硅20制作真空袋

概述


Overview
EZ~Spray® Silicone 20 Spray Rubber is made especially for dispensing through the EZ~Spray® Jr. Spray Gun, this silicone is softer (Shore 20A) and stronger vs. our original EZ~Spray® Silicone.

Based on our Dragon Skin® silicone technology, this spray rubber is an exceptional mold material and offers higher physical properties than our original EZ~Spray® Silicone rubber (we will continue to offer EZ~Spray® silicone rubber, renamed EZ~Spray® Silicone 35).

EZ~Spray® Silicone 20 is also good for making custom spray vacuum bags and offers several advantages over vacuum bags made using conventional methods. EZ~Spray Silicone 20 bags conform perfectly to your tool, meaning perfect parts every time. Silicone vacuum bags are also virtually indestructible and stand up to high temperatures. Perfect for pre-preg, wet-preg and infusion processing. One of the biggest advantages, due to the fact that silicone bags are re-usable, is the time and labor savings realized if there are more than 6 parts to be made - up to 80% savings vs. conventional vacuum bags.

Materials Used in this Tutorial Step 1: Making Vacuum Bag
Spray the EZ~Spray® Silicone 20 over the tool and remove the cured vacuum bag.





Step 2: Preparing the Bag
Lay up the composite material and reposition the vacuum bag.






Step 3: Casting and Finishing
Use the vacuum to create the part. The finished composite hood created by Vermont SportsCar Rallying - www.vtcar.com