URE-FIL® 5

URE-FIL® 5

Smooth-On URE-FIL®填充剂可轻松分散在Smooth-On材料中。它们可以以不同比例添加到材料中,以实现各种工作特性和效果。一些填充剂是为了节约成本而设计,一些填充剂是为特定的浇注效果或改进物理性能而设计,一些UREFIL®填充剂专为增稠材料而设计,用于刷涂或镘涂应用场合。
 
URE-FIL®5是制作木纹效果的最佳选择。注意:模具必须具有原始模型的木纹图案。将1份填料与1A : 1B的Smooth-Cast320树脂混合并浇注到模具中。脱模后,将木色着色剂或鞋油涂在浇注件表面,以显示木纹效果。

特征

说明

URE-FIL® fillers must be thoroughly dispersed in liquid rubber or resin to a uniform consistency. When adding large concentrations of filler, it is recommended to add the filler to completely mixed rubber or resin - combine both parts A and B of rubber or resin, mix throughly, then add filler. Mix the filler in and confirm that there are no lumps of filler present. Often, employing the ‘double-mix and pour’ technique can produce better results.
 

Guarding Against Moisture - All powder fillers will absorb atmospheric moisture over time which will react with urethane materials. If you experience bubbling or foaming in your resin/filler mix, your filler probably contains moisture.

Remedy: Line a cookie sheet with foil and spread filler evenly over the cookie sheet at 3/8”-1/2” thickness (0.95 cm-1.25 cm). Place in an oven on warm setting (100°F / 38°C) and bake for two hours. Remove cookie sheet from oven (don’t burn yourself!) and redistribute filler on cookie sheet. Place back in oven and bake for two hours. Let filler cool to room temperature before mixing with urethane materials.

Storage - To prevent moisture absorption, use filler as quickly as possible after purchasing. Decant filler from container and replace lid immediately...do not leave container opened for more than a minute. If filler will be stored for prolonged periods, obtain dessicant pouches at your local hobby/arts and crafts store and place one or two dessicant pouches in container. Replace used dessicant pouches every other time you open container. Make sure container lid is secure before storing.

介绍产品制作工艺的文章

木纹饰面效果的模具制作和浇注

木纹饰面效果的模具制作和浇注

视频演示Smooth-Cast320浇注在Dragon Skin硅胶模具中,复制木纹效果