Sil-Poxy™

Sil-Poxy™

Sil-Poxy™为单组分硅胶粘合剂,专门用于粘合Smooth-On的RTV模具制作硅胶与硅胶和其他基材,包括一些塑料(聚氨酯)、石膏/陶瓷、织物等。
 
Sil-Poxy™用于锡固化或铂固化硅胶粘合,提供具有高伸长率粘合。硅胶部件之间粘合牢固而具有柔性。可以用Silc-Pig™硅胶颜料着色。固化后的硅胶粘合剂可耐风化、潮湿、紫外线和高温。
 
Sil-Poxy™硅胶粘合剂可用于修复撕裂的硅胶模具。其他应用包括用于假肢和电子动画的硅胶粘合

特征


说明

Safety - Use in a properly ventilated area (“room size” ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk.

Store and use material at room temperature (73°F/23°C). This product has a limited shelf life and should be used as soon as possible.

A clean, dry surface is essential for successful adhesive bonding. If possible, abrade surface and follow with solvent wipe before applying.

Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.

Dispensing - Squeeze tube, taking care not allow air to enter tube before replacing cap. Unused product in tube exposed to air will cure quickly.

Applying - Apply adhesive to surface and mate parts. Material will begin to cure in 15 minutes. Pieces can be handled after 1 hour. Full cure is attained after 24 hours. Warmer temperatures (and higher humidity) will result in a faster cure. Lower temperature will retard cure.