Safety - Use in a properly ventilated area (“room size” ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk.
Store and use material at room temperature (73°F / 23°C). This product has a limited shelf life and should be used as soon as possible.
Measuring - When used alone as Part B for Mold Max® 30 (100A:10B pbw mix ratio) instead of regular catalyst, Fast Cat® 30 reduces the pot life of Mold Max® 30 from 45 minutes to 10 minutes and the demold time from 24 hours to 1 hour. If the amount of Fast Cat® 30 Part B is increased to 15% (100A:15B pbw), the pot life is reduced to 5 minutes and the demold time to 30 minutes.
Mixing - Add desired amounts of Fast Cat® 30 and/or regular Mold Max® 30 Part B to Mold Max® 30 Part A by weight and mix thoroughly. Important: Be sure to scrape the sides and bottom of the mixing container several times while mixing. Be aware of your working time with reduced pot life. Note: results may differ due to variables in temperature, humidity, etc.
Note: Working time is reduced in proportion to the amount of Fast Cat® 30 added. Adding Fast Cat® reduces the library and production life of the cured rubber vs. our Mold Max® regular catalyst