使用Habitat Black制作真实尺寸的龙

Making a Life Size Dragon Using Habitat® Black

How do you sculpt a realistic dragon, let alone one that has to be life size? That's what effects artist Frank Ippolito did for Capcom's booth at this year's E3 gaming conference. We visit Frank's shop before the event to see the in-progress dragon--the Gore Magala from the game Monster Hunter 4 Ultimate--before it's brought to life and then behold the impressive finished piece on the E3 show floor.