SuperSeal®

SuperSeal®

SuperSeal®为经济、快干的密封剂,适用于各种多孔表面,包括石膏灰泥、混凝土和木材。密封剂可快速有效地密封表面而不干扰表面细节。新配方具有更好的性能和更快的蒸发速度,封闭后使用模具橡胶(聚氨酯,硅树脂或聚硫化物)。

特征


说明

Safety - CONTENTS FLAMMABLE: Keep product away from flame and all ignition sources. Use in a properly ventilated area (“room size” ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk.
 

Store and use material at room temperature (73°F/23°C). This product has a limited shelf life and should be used as soon as possible.


NOTE: ALWAYS SHAKE WELL BEFORE USING

A minimum of 2 coats of SuperSeal® is recommended to seal most surfaces. For extremely porous surfaces (i.e. limestone or dry plaster) an additional coat of SuperSeal® may be required. Or apply two coats of SuperSeal® and follow with an application of Ease Release® 200. Superseal® can be applied using a soft brush or a non-aerosol spray bottle to lightly mist SuperSeal® onto model.

  1. Apply a thorough thin coating of SuperSeal® over entire model surface and surrounding forms including intricate detail and undercuts. Compressed air or a hair dryer may be used to blow off any excess that has pooled. Let dry for 5 minutes.
  2. Repeat above 1 - 2 more times and let final coat dry for at least 1 hour.
  3. If recommended by mold rubber manufacturer, apply a light mist coating of release agent (i.e. Ease Release® 200). Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.

Important: Discoloration of model surface may occur. If compatibility between SuperSeal® and model surface or SuperSeal® and a particular mold rubber is a concern, a small-scale test should be made on an identical surface prior to use.