SO-Strong®着色剂高浓缩,具有优异的分散性,颜色一致性。非常少的用量即可成比例着色大量液体聚氨酯材料。按液体聚氨酯体积比例添加越多,颜色效果就越显着。推荐的添加范围是系统总重量的0.01%至3%。液体聚氨酯系统中不能过多添加,可能出现抑制固化/渗出。
用户决定添加的数量; 如果是第一次在聚氨酯系统中添加色彩或颜料,可能需要通过向少量聚氨酯材料添加几滴颜色来测试颜色效果,并观察结果。可能需要几个测试浇注件才能达到所需的颜色效果。
色彩:黑色,黄色,棕色,紫色,绿色,橙色,红色和蓝色。
彩色颜料:白色和肉色
By Weight Using A Gram Scale: Add SO-Strong®colorant at a ratio of between 0.01% - 3% of the total weight (Parts A + B mixed) of the material being cast. Adding more than 3% by weight may cause cure inhibition.
By Volume Measured In Drops: Add 10 drops of SO Strong® per 3 oz (88 ml) of mixed urethane material. If using a translucent material (like Smooth-Cast® 325) you can use 1 drop to maintain translucency of the material.
Directions For Use: Store and use at 73°F / 23°C. Wear vinyl gloves to prevent skin contact. After dispensing the required amount of urethane material Parts A and B into measuring containers, add colorant to Part B and mix thoroughly. Combine Parts A and B into a mixing container and mix as directed by the urethane product technical bulletin.
Blending Colors: Combine different colors on a palette to create a custom color before adding to material as directed above.
The Pantone Color Matching System is most commonly used in the printing industry to communicate color. As it relates to Smooth-On color tints and pigments, the represented color is an approximation and people’s interpretation of these colors may vary. The user will determine suitability of a color or combination of colors for the rubber, resin, foam or other product used specifically for their application. Due to the variability in products that are being colored, application, color concentration and other factors, Smooth-On makes no warranty with regards to the color.