PoYo™ Putty 40 is a two-component mold making silicones (tin catalyst) that can be mixed and applied “on site” – directly to almost any model. PoYo™ Putty will hold any vertical surface and capture even the finest detail - perfect for making strong rubber molds that can be used within minutes. Use Less – Do More: Because PoYo™ is applied as a thin layer, less material is used, saving you money. Molds are also lightweight, making them easier to handle.

PoYo™ Putty has been used to make molds of valuable antiques and archeological models and can be used to make fast molds of sculpture, prototypes, candles, picture frames, coins, etc. You can cast wax, gypsum and a variety of resins into PoYo™ Putty molds.

In this example, PoYo™ is used to mold the detail of natural tree bark, resulting in a mold which can be used to cast resin, plaster, even foam!

Materials Used in this Tutorial Step 1: Mixing PoYo Putty
PoYo putty has a mix ratio of 20:1 by volume. (Think golf ball:marble) To combine, fold the PoYo putty onto itself until an even color is achieved.







Step 2: Applying PoYo
Next, apply the PoYo directly to the bark of a large tree. After 30 minutes at 73F/23C, the mold is cured and can be removed.





Step 3: Casting with Smooth-Cast 320
Now, pour pigmented Smooth-Cast 320 into mold, this results in a perfectly detailed casting.