Quarry Tone®

Quarry Tone®

QuarryTone®花岗岩特效填料为特殊混合粉末,可添加到一些Smooth-Cast®液体塑料或液体橡胶中,制作逼真石材效果成品浇注件。有10种花岗岩效果粉末可供选择,每种都有自己的粒度和颜色。
 
为了获得最佳效果,请使用QuarryTone®粉末和快速固化的半透明树脂,例如Smooth-Cast®325。快速固化树脂可在整个成品浇注件中实现均匀填料分散。如果树脂系统太慢,填料可能在成品浇注件中不均匀地沉降。QuarryTone®粉末也可添加到半透明/透明硅胶中,例如DragonSkin®或EcoFlex®系列,用于制作柔软和柔韧的花岗岩状道具。QuarryTone®粉末也可以混合,制作其它成品效果。

特征

可用于透明树脂或橡胶

说明

Pre-mix before dispensing. Store and use all materials at or near 73°F/23°C. Quarry Tone® fillers must be kept dry. Use with adequate ventilation. Read and follow directions for resin used to mix with Quarry Tone® fillers. The following example features Smooth-Cast® 325 (A+B) mixed with Quarry Tone® powder. The powder must be thoroughly dispersed into a two component liquid resin or rubber to a uniform consistency.
 

Recommended Mix Ratio by Volume:

1A + 1B + 2 Parts Powder Filler.

By Volume Mixing & Casting Procedure:

  1. Dispense 1 cup of Smooth-Cast® 325 Part B into a clean mixing container.
  2. Dispense 2 cups Quarry Tone® powder into mixing container.
  3. Mix thoroughly.
  4. Dispense 1 cup of Smooth-Cast® 325 Part A into mixing container.
  5. Mix for 30 seconds until all filler particles are dispersed and pour into rubber mold.

Guarding Against Moisture – All powders will absorb atmospheric moisture over time which will react with urethane resins. If you notice a moisture reaction between resin and powder or suspect that your Quarry Tone® powder contains moisture, you can remedy by spreading powder evenly over a metal cookie sheet at ¼” (0.6 cm) thickness and bake in oven for 4 hours at 150° F/60° C. Allow to cool before mixing powder with resin. Store powder tightly closed container in a cool, dry environment with a desiccant pouch (available at your local hobby/arts and crafts store). Replace used desiccant pouches every other time you open container.