SLIDE® STD

SLIDE® STD

SLIDE®STD表面张力分散剂为铂金固化硅胶添加剂,制作表面张力大大降低的固化硅胶产品。固化硅胶可在其自身和不同表面上滑动。SLIDE®STD按B组分的百分比添加。硅胶表面必须暴露在空气中24小时才能产生滑动效果。
 
由于其超低的表面张力,SLIDE®STD非常适合制作硅胶面罩等。使用SLIDE®STD制做的硅胶浇注件表面具有非常低的摩擦力,浇注硅胶件需要在像皮肤表面滑动时,移动方便。
 
硅胶会随着时间而变黄。如果不希望变黄,混合前在液体硅胶中加入Silc Pig®有机硅颜料,对硅胶着色。
 
警告 - 过敏原: 对榴莲、树坚果和树坚果衍生物或麝香蓟种子过敏的人应避免与本产品接触。

特征

说明

Safety - Use in a properly ventilated area ("room size" ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk. Wear vinyl gloves only. Latex gloves will inhibit the cure of the rubber. Store and use material at room temperature (73ºF/23ºC). Warmer temperatures will drastically reduce working time and cure time. Storing material at warmer temperatures will also reduce the usable shelf life of unused material. These products have a limited shelf life and should be used as soon as possible.
 

Measuring & Mixing - SLIDE® STD is added by weight to Part B and should be thoroughly mixed into Part B before adding Part A. An accurate gram scale must be used. Calculate the correct amounts of Part A, Part B and SLIDE® STD in advance.

  1. Weigh out the required amount of Part B.
  2. Weight out and add up to 1.5% of SLIDE® STD as a percentage of the Part B. Mix Part B and SLIDE® STD thoroughly.
  3. Weigh out and add the required amount of Part A.
  4. Mix thoroughtly, eliminating all color streaks from the mixture.
  5. Pour mixture into new, clean mixing container and mix again.
  6. Pour rubber into containment field or mold.

Low Surface Tension Properties - In order for SLIDE® STD to exhibit it's ultra-low tension properties, the silicone surface must be exposed to air for at least 24 hours. After material cures for 16 hours, demold immediately and position the casting in such a way that all surfaces comes into contact with air. This will allow the material to develop a very low-friction surface.

Adhesion and Lamination - Once SLIDE® STD have developed its ultra-low surface tension properties, other platinum silicones (Psycho Paint®, Dragon Skin®, EcoFlex®, etc.) will not bond to a cured piece. in order to bond another silicone to a casting made using SLIDE® STD (painting with Psycho Paint®, for example) the new silicone must be applied before silicone with SLIDE® STD added develops it's low-friction surface.

Use In a Mold Material - Silicone molds created with SLIDE® STD are adhesive when casting urethane resins and other materials. If you use SLIDE® STD in your mold material, applying a release is necessary before casting.