HYPER-FOLIC™脱模添加剂为无毒皮肤调理剂,在将硅胶涂在皮肤上之前与Body Double™硅胶模具橡胶混合。
 
HYPER-FOLIC ™不仅有助于将固化硅胶从皮肤上脱模,还可以从毛发覆盖的皮肤表面(紧密的胡须、胡须、眼眉、阴毛等)脱模

特征

优点:


说明

PREPARATION:
 

Usage Example - 50 grams of Body Double™ FAST SET part A and 50 grams of Body Double™ FAST SET part B are weighed into separate containers using a gram scale. 20 grams of HYPER-FOLIC™ is added to Body Double™ part B and thoroughly mixed. Body Double™ part A is combined with the Body Double™ part B / HYPER-FOLIC™ in a larger mixing container and is mixed thoroughly. This mixture is then applied to the skin surface directly.


Usage Option #1 - Mix HYPER-FOLIC™ with Body Double™ rubber components at a 100A + 100B + 40 Parts HYPERFOLIC™ ratio by weight (20% HYPERFOLIC added to the silicone by weight) and apply.

Results – Body Double™ mold rubber will completely penetrate facial or body hair and capture detail from underlying skin. Hair detail will mostly not be reflected in the finished mold or reproduced during casting. This technique is often used for prosthetic make-up applications.

Usage Option #2 - Apply Body Double™ Release Cream liberally to the skin and facial or body hair. Mix HYPER-FOLIC™ at a reduced amount with Body Double™ rubber components at a 100A + 100B + 20 Parts HYPER-FOLIC™ ratio by weight (10% HYPERFOLIC added to the silicone by weight) and apply.

Results – Body Double™ mold rubber will partially penetrate hair and hair detail will be reflected in the finished mold or reproduced during casting.


USAGE TIPS


How Does HYPER-FOLIC™ additive affect Body Double rubber?


Casting Into The Finished Mold - You can cast a variety of materials into the finished mold without a release agent including wax, plaster, concrete, resins, etc. Using a release agent (such as Ease Release™ 200) for production casting of resins will extend the production life of the mold.