Directions for Use – Pre-mix all liquid resin, rubber or foam before dispensing. Store and use all materials at or near 73°F/23°C. Glow Worm® powders must be kept dry (see ’Guarding Against Moisture’ section). Use with adequate ventilation. Read and follow directions for material used to mix with Glow Worm® powders. The following example features SmoothCast® 325 (A+B) mixed with Glow Worm® powder. The powder must be thoroughly dispersed into a two component liquid resin or rubber to a uniform consistency.
Recommended Mix Ratio by Volume: 1A + 1B + 1 Part Glow Worm® powder.
By Volume Mixing & Casting Procedure:
Lower Your Cost Per Casting - Glow Worm Powders are Expensive: Mix small amounts as directed above and brush layers into a mold to coat the mold cavity (known as a face coat or gel coat).
Optional: Combine Smooth-Cast®/Glow Worm® mixture with 1 part Ure-Fil® 11 to increase brushability of gel coat. Follow by backfilling with straight resin or foam.
The glow effect will be the same vs. a solid casting and material cost will be greatly reduced.
Guarding Against Moisture – All powders will absorb atmospheric moisture over time which will react with urethane resins. If you notice a moisture reaction between resin and powder or suspect that your Glow Worm® powder contains moisture, you can remedy by spreading powder evenly over a metal cookie sheet at ¼” (0.6 cm) thickness and bake in oven for 4 hours at 150° F/60° C. Allow to cool before mixing powder with resin. Store powder in a tightly closed container in a cool, dry environment with a desiccant pouch (available at your local hobby/arts and crafts store). Replace used desiccant pouches every other time you open container.
Glow Worm® Powders are up to 50% brighter than the competition.