PC-3®实验室台面粘合剂为双组分黑色环氧树脂粘合剂,设计用于连接、粘结和填塞实验室柜台和桌子。环氧树脂粘合剂填充量大,粘附在垂直表面上不会下垂。它在室温下固化,收缩率极低。

特征

PC-3®不含挥发性有机化合物(VOC)或溶剂。耐溶剂和稀的酸,与天然/人造石材、大多数金属、玻璃、木材以及热固性树脂(如聚酯酚醛树脂和环氧树脂)结合牢固。PC-3®采用品脱单位包装(2.5磅)或夸脱单位包装(5.0磅),仅按箱销售。品脱箱包含6个,夸脱箱包含3个

PC-3® Coverage Rates 1/16” (1.59 mm) thick 1/8” (3.18 mm) thick 1/4” (6.35 mm) thick 3/8” (9.53 mm) thick
Pint Unit: 2.5 lbs (1.14 kg) 5.56 ft2 (.516 m2) 400 in2 (2581 cm2) 200 in2 (1290 cm2) 133 in2 (860 cm2)
Quart Unit: 5 lbs (2.28 kg) 11.1 ft2 (1.03 m2) 800 in2 (5161 cm2) 400 in2 (2581 cm2) 266 in2 (1716 cm2)

说明

Safety - Use in a properly ventilated area (“room size” ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk.
 

Store and use material at room temperature (73°F/23°C). This product has a limited shelf life and should be used as soon as possible.

Any surface to which the PC-3® will be applied should also be at least 73°F/23°C. Sand surface and wipe clean with fast drying solvent (such as acetone) prior to applying PC-3®. Surface must be clean, dry, and free of all contaminants such as oil, grease, water, dust, etc. Mask adjacent areas with masking tape, then strip tape off as soon as installation is completed. Remove excess or unwanted cement with solvent before it sets.

Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.


Measuring & Mixing - It is important that Parts A & B be mixed accurately in equal amounts. Excess amounts of either Part A or B will cause improper curing of the material. After dispensing equal amounts of Parts A & B, mix thoroughly for 5 minutes, making absolutely sure that you scrape the sides and bottom of the mixing container several times. If you notice streaks in the mixed material, it is not mixed thoroughly enough. Normal cure time is 24 hours.