Ease Release® 2831

 Ease Release® 2831

Ease Release®2831为蜡基非有机硅脱模剂。已被证明有效用于聚氨酯发泡弹性体脱模。Ease Release®2831适用于铝、钢和弹性体模具结构。

特征


说明

Safety - Use in a properly ventilated area (“room size” ventilation). Wear safety glasses, long sleeves and rubber gloves to minimize contamination risk. Skin contact may cause dryness.
 

Store and use material at room temperature (73°F/23°C). This product has a limited shelf life and should be used as soon as possible.


SHAKE WELL BEFORE USING

Applying - Apply a coat of Ease Release® 2831 with a spray or brush, and allow to dry. Rub Ease Release® 2831 into mold surface with a clean cloth. Repeat two or three times to seal the mold surface. Start molding and reapply a light coat of Ease Release® 2831 after each molding cycle.

Finishing - Thorough cleaning of the molded parts is recommended prior to bonding or any other post mold finishing.

介绍产品制作工艺的文章

制作定制发泡储存嵌块

制作定制发泡储存嵌块

定制发泡嵌块用于电子或其它精密设备

› 查看介绍文章