AquaCon®

AquaCon®

AquaCon水性混凝土脱模剂帮助混凝土浇筑件从Smooth-On橡胶模具和其它表面(如三聚氰胺板、金属和无孔隙封闭过的木材)脱模。产品提供干净、真正脱模效果,不影响颜色和表面细节,并且有助于将成品浇注件的斑眼和气泡降至最低。

特征

涂布率-薄膜(0.013mm)厚,1加仑未稀释的脱模剂可以涂297m2.

说明

PREPARATION... Safety - Wear safety glasses to minimize contamination risk. Store and use at room temperature (73°F/23°C). Do not use below 45°F/8°C.
 

Pre-Mixing - Before dispensing, shake container or stir thoroughly with a paddle or drill mixer set on a slow speed to a uniform consistency.

Diluting AquaCon® - AquaCon® can be used straight or diluted with up to 8 parts water. The dilution ratio depends on your concrete mix design. Finding the right balance between AquaCon® and water can affect bug holes. If using on a new rubber mold, it is recommended that AquaCon® be used straight (undiluted) for each casting for the first 10 castings. 1 – 10 castings, use undiluted. After 10 castings, dilute 1 part AquaCon® : 4 Parts Water After 20 castings, dilute 1 part AquaCon® : 8 Parts Water Mix only amount needed for one day. Mixture may separate in the container after a few hours. Before dispensing, pre-mix before to a uniform consistency.

Applying - Coat mold surface with a very thin film (.0005 in / .013 mm). Apply with a brush, roller, HVLP gun or Kwikee® Sprayer. Do not allow release agent to pool in the mold. Wipe over mold surface using a clean, soft cloth.

Caution: Do Not Over Apply. Applying too much release agent will cause air bubbles “wormtracks”, “bugholes” or pitting on surfaces. After applying AquaCon to mold surface, you can mix and cast concrete immediately.

Mix only amount needed for one day. Mixture may separate after 24 hours. Re-mix to a uniform consistency and apply. Because no two applications are quite the same, a small test application to determine suitability for your project is recommended if performance of this material is in question.

介绍产品制作工艺的文章

使用Aquacon水性混凝土脱模剂浇注混凝土

使用Aquacon水性混凝土脱模剂浇注混凝土

AquaCon水性混凝土脱模剂用于混凝土从smooth-on橡胶模具中脱模

› 查看介绍文章

使用GFRC制作定制混凝土台面

使用GFRC制作定制混凝土台面

了解如何使用Forton VF-774制作特别坚固的混凝土台面

› 查看介绍文章